| You are the site ¡ú Products ¡ú Saturable
Nanorystalline Cores For MAG-AMP£¨FUH£© |
| |
Saturable Nanorystalline Cores
For MAG-AMP£¨FUH£© |
 |
Features£º |
| ¡ó Low coercive force and high squareness ratio |
| ¡ó High saturation magnetic induction Bs |
| ¡ó Low core losses |
| ¡ó Extended temperature rang up to 120¡æ |
| ¡ú reduction of weight, volume and cost |
| |
| Applications£º |
| ¡ó Magnetic amplifier for switched mode power
supply |
| ¡ó Magnetic amplifier for DC to DC converter |
| ¡ó ATX computer, micro ATX computer |
| ¡ó Other kinds of saturable reactor |
|
| |
 |
|
|
| |
| Properties£º |
| |
FUH |
The cobalt base amorphous
(can be saturated) |
Ferrite |
| saturation Bs£¨T£© |
1.21 |
0.54 |
0.37 |
| Rectangular
ratio Br/Bs |
0.85 |
0.85 |
0.5 |
Coercivity
Hc (A/M)
|
0.70 |
0.60 |
30 |
| Curie temperature
Tc (¡æ) |
550 |
200 |
170 |
| Core loss P2/100K
(kW/M3) |
800 |
450 |
650 |
|
| |
| Specifications£º |
¡¡¡¡
| Grade |
Finished dimension
(mm)OD ID H |
Core dimension
(mm)OD ID H |
Section(mm2) |
Length of average
magnetism way(mm) |
Total flux2§æm(¦ÌWb) |
Rectangular ratio
(Br/Bs)
f=100kHz |
| FUH7¡Á4¡Á3 |
9.2 3.2 4.8 |
7 4.0 3.0 |
3.38 |
18.8 |
8.11 |
¡Ý0.92 |
| FUH8¡Á4.5¡Á5 |
9.0 3.5 7.2 |
8 4.5 5.0 |
6.56 |
19.6 |
15.74 |
FUH10¡Á6.5¡Á4.5
|
11.3 5.1 6.6 |
10 6.5 4.5 |
5.90 |
25.9 |
14.16 |
| FUH12¡Á8¡Á4.5 |
13.9 6.7 6.6 |
12 8.0 4.5 |
6.75 |
31.4 |
16.20 |
| FUH14¡Á10¡Á5 |
15.9 8.8 7.2 |
14 10 5.0 |
7.50 |
37.6 |
18.00 |
| FUH18¡Á12¡Á4.5 |
19.8 10.8 6.6 |
18 12 4.5 |
10.12 |
47.1 |
24.28 |
| FUH21¡Á14¡Á4.5 |
22.8 12.8 6.6 |
21 14 4.5 |
11.80 |
55.0 |
28.32 |
|
| |
|
 |
|
|
|
|
|
| Add:Xiaoying Eaet Rd,Haidian District,Beijing
100085, China |
| Postal code:100085 |
| Tel:0086-10-62949563,62957217 |
| Fax:0086-10-62925648 |
| Linkman:Mr.Tu Mr.Pang Mr.Ji |
| http://www.bj-shouye.com |
| E-mail:sales@shouye.sina.net |
|
|
|